Material Notes:
Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than 440C. For knife makers, it offers better edge retention than 440C. It also has higher attainable hardness and better through hardening characteristics than 440C.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58.5
58.5
Modulus of Elasticity 207 GPa
30000 ksi
Thermal Properties Metric English Comments
CTE, linear 7.02 µm/m-°C

@Temperature -73.3 - 21.1 °C
3.90 µin/in-°F

@Temperature -100 - 70.0 °F
10.35 µm/m-°C

@Temperature 21.0 - 149 °C
5.750 µin/in-°F

@Temperature 69.8 - 300 °F
10.91 µm/m-°C

@Temperature 21.0 - 260 °C
6.061 µin/in-°F

@Temperature 69.8 - 500 °F
11.86 µm/m-°C

@Temperature 21.0 - 482 °C
6.589 µin/in-°F

@Temperature 69.8 - 900 °F
Thermal Conductivity 24.2 W/m-K

@Temperature 95.0 °C
168 BTU-in/hr-ft²-°F

@Temperature 203 °F
Component Elements Properties Metric English Comments
Carbon, C 1.05 %
1.05 %
Chromium, Cr 14 %
14 %
Iron, Fe 80.95 %
80.95 %
As Remainder
Molybdenum, Mo 4.0 %
4.0 %
Descriptive Properties Value Comments
Total Carbide Volume; % 17.5
Wear Resistance; mg 49
Pin abrasion method