Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Vexel™ E20GF15 , 15% Glass Reinforced PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 20% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ E20GF15 , 15% Glass Reinforced PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ E20GF15 is a 15% glass fiber reinforced, general purpose PET. Information provided by Custom Resins.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 114 MPa
16500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Modulus 4.96 GPa
720 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648
Users viewing this material also viewed the following: