Custom Resins Vexel™ E20GF30 FR , 30% Glass Reinforced, Flame Retardant PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ E20GF30 FR , 30% Glass Reinforced, Flame Retardant PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ E20GF30 FR is a 30% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
420 °F
ASTM D648
Users viewing this material also viewed the following: