Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Cytec
Trade Name Conathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.Cytec (Conap) CE-1164 Conathane® Polyurethane Dielectric Conformal CoatingSingle ComponentPasses Thermal Shock Test (MIL-I-46058C)Non-Nutrient Fungus Resistance (MIL-I-46058C)Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)Very Good Chemical and Solvent ResistanceMoisture Cure (must have a minimum of 30% relative humidity to fully cure) Cure Type: Moisture
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity 150 cP

@Temperature 25.0 °C
150 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 54.4 °C
130 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Flash Point 12.8 °C
55.0 °F
(TCC)
Electrical Properties Metric English Comments
Electrical Resistivity 4.50e+12 ohm-cm
4.50e+12 ohm-cm
Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity)
2.50e+13 ohm-cm
2.50e+13 ohm-cm
Initial Insulation Resistance (50% Relative Humidity)
1.30e+10 ohm-cm

@Temperature 65.0 °C
1.30e+10 ohm-cm

@Temperature 149 °F
Insulation Resistance During 10th day Cycling (95% Relative Humidity)
Dielectric Constant 2.7
2.7
ASTM D150
Dielectric Strength 138 kV/mm
3500 kV/in
ASTM D149
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Cure Time 20.0 - 30.0 min

@Temperature 25.0 °C
0.333 - 0.500 hour

@Temperature 77.0 °F
tack free
240 min

@Temperature 60.0 °C
4.00 hour

@Temperature 140 °F
10080 min

@Temperature 25.0 °C
168.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month