Material Notes:
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.Cytec (Conap) EN-2532 Potting and Encapsulation AdhesivePasses Thermal Shock Test (10 Cycles, -65°C to 130°C)Non-Nutrient Fungus Resistance (MIL-STD-810B)Mix Ratio: 20/100 (by Weight)
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Cured
Water Absorption 0.20 %
0.20 %
24 hours
Water Absorption at Saturation 0.0055 %
0.0055 %
30 Days
Viscosity 4000 cP

@Temperature 25.0 °C
4000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 70 - 75
70 - 75
Tensile Strength, Ultimate 20.7 MPa
3000 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.272 W/m-K
1.88 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.60e+14 ohm-cm
<= 1.60e+14 ohm-cm
Surface Resistance 4.60e+13 ohm
4.60e+13 ohm
Dielectric Constant 3.86

@Frequency 1000 Hz
3.86

@Frequency 1000 Hz
Dielectric Strength 23.0 kV/mm

@Thickness 1.59 mm
585 kV/in

@Thickness 0.0625 in
Dissipation Factor 0.044

@Frequency 1000 Hz
0.044

@Frequency 1000 Hz
Arc Resistance >= 120 sec
>= 120 sec
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 100 °C
2.00 hour

@Temperature 212 °F
960 min

@Temperature 80.0 °C
16.0 hour

@Temperature 176 °F
10080 min

@Temperature 25.0 °C
168.0 hour

@Temperature 77.0 °F
Pot Life 15.0 - 20.0 min

@Temperature 25.0 °C
15.0 - 20.0 min

@Temperature 77.0 °F
1 lbm
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: