Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer Cytec
Trade Name Thornel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 970 MPa
141000 psi
Tensile Modulus 470 GPa
68200 ksi
Compressive Yield Strength 290 MPa
42100 psi
Shear Strength 35.0 MPa
5080 psi
Thermal Properties Metric English Comments
Thermal Conductivity 321 W/m-K
2230 BTU-in/hr-ft²-°F