DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Mineral Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
(DAM); ISO 1183
Water Absorption 6.2 %
6.2 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
DAM; ISO 294-4
0.0050 cm/cm
0.0050 in/in
DAM; ISO 294-4
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Comparative Tracking Index >= 600 V
>= 600 V
PLC 0; UL 746A
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Heat stabilized or stable to heat Yes
Injection molding Yes
Release Agent Yes
RSV Formic Acid 2.25 g/100ml
ISO 307
With Fillers Yes
Users viewing this material also viewed the following: