DSM Akulon® XG-FKGS6 PA6-GF30 FR

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® XG-FKGS6 PA6-GF30 FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced, Flame Retardant, Halogen free
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
dry; ISO 1183
Moisture Absorption 1.70 %
1.70 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
cond; ISO 527-1/-2
135 MPa
19600 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
3.7 %
3.7 %
cond; ISO 527-1/-2
Tensile Modulus 7.10 GPa
1030 ksi
cond; ISO 527-1/-2
11.5 GPa
1670 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
dry; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
IEC 60695-11-10
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
Glow Wire Test 775 °C

@Thickness 1.60 mm
1430 °F

@Thickness 0.0630 in
Glow Wire Ignition Temperature; IEC 60695-2-13
775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
Glow Wire Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 1.60 mm
1760 °F

@Thickness 0.0630 in
Glow Wire Flammability Index, dry; IEC 60695-2-12
960 °C

@Thickness 0.800 mm
1760 °F

@Thickness 0.0315 in
Glow Wire Flammability Index, dry; IEC 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
cond; IEC 60112