Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnitel® XG5855 TPC-ET

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® XG5855 TPC-ET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion Grade
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 0.17 %
0.17 %
Sim. To ISO 62
Moisture Absorption 0.450 %
0.450 %
Sim. To ISO 62
Melt Flow 2.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 86

@Time 3.00 sec
86

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 8.50 MPa
1230 psi
ISO 527-1/-2
Tensile Stress 3.00 MPa

@Strain 10.0 %
435 psi

@Strain 10.0 %
ISO 527-1/-2
4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 350 %
350 %
ISO 527-1/-2
Tensile Modulus 0.0560 GPa
8.12 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 172 °C
342 °F
10°C/min; ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+13 ohm-cm
1.90e+13 ohm-cm
IEC 60093
Dielectric Strength 21.0 kV/mm
533 kV/in
IEC 60243-1
Copyright © lookpolymers.com All Rights Reserved