Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ISO 868
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ISO 527
Elongation at Break 270 %
270 %
ISO 527
Modulus of Elasticity 1.512 GPa
219.3 ksi
ISO 527
Flexural Modulus 1.712 GPa
248.3 ksi
ISO 178
Shear Modulus 0.700 GPa
102 ksi
torsional
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180, Ductile break
9.00 kJ/m²

@Temperature -40.0 °C
4.28 ft-lb/in²

@Temperature -40.0 °F
Brittle break; ISO 180
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
DIN 53453, Ductile break
1.40 J/cm²

@Temperature -40.0 °C
6.66 ft-lb/in²

@Temperature -40.0 °F
Brittle break; DIN 53453
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
DSC