DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer DSM Fibre Intermediates
Trade Name Nyrim®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.321 g/cc
0.04772 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Ultimate 22.0 MPa
3190 psi
ISO 527
Elongation at Break 50 %
50 %
ISO 527
Modulus of Elasticity 1.75 GPa
254 ksi
ISO 527
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DIN 53453
0.500 J/cm²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
DIN 53453