DSM Stanyl® TE263F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Impact Modified (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TE263F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Impact Modified (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
(DAM); ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527-1/-2
Elongation at Break 10 %
10 %
ISO 527-1/-2
Flexural Modulus 3.20 GPa
464 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
(DAM); ISO 11357-1/-3