Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TW241F5 PA46-GF25

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW241F5 PA46-GF25.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Stabilized, 25% Glass Reinforced
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
dry; ISO 1183
Moisture Absorption 2.80 %
2.80 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 180 MPa
26100 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
Tensile Modulus 9.00 GPa
1310 ksi
dry; ISO 527-1/-2
Flexural Modulus 7.50 GPa
1090 ksi
dry; ISO 178
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
dry; ISO 75-1/-2
Users viewing this material also viewed the following: