DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
(DAM); ISO 1183
Water Absorption 13.5 %
13.5 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 3.7 %
3.7 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
DAM; ISO 294-4
0.020 cm/cm
0.020 in/in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 500 MPa
72500 psi
ISO 899-1
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min (DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
IEC 60250
22

@Frequency 100 Hz
22

@Frequency 100 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60243-1
Dissipation Factor 0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
IEC 60250
0.087

@Frequency 100 Hz
0.087

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 400 V
400 V
IEC 60112
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
Injection molding Yes
Lubricants Yes
Platable Yes
Release Agent Yes
Without Fillers Yes