Material Notes:
NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can be obtained.Description: Aqueous.Major Uses:Coating, casting.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
at 25°C
Solids Content 40 %
40 %
Oxygen Transmission 320 cc-mm/m²-24hr-atm
812 cc-mil/100 in²-24hr-atm
at 25°C
Nitrogen Transmission 104 cc-mm/m²-24hr-atm
263 cc-mil/100 in²-24hr-atm
at 25°C
Viscosity 3.0 - 7.0 cP
3.0 - 7.0 cP
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
FEP Component
Oxygen Index >= 95 %
>= 95 %
FEP Component
Electrical Properties Metric English Comments
Dielectric Constant 2.0 - 2.2

@Frequency 1000 Hz
2.0 - 2.2

@Frequency 1000 Hz
FEP Component; ASTM D150
2.0 - 2.2

@Frequency 1e+6 Hz
2.0 - 2.2

@Frequency 1e+6 Hz
FEP Component; ASTM D150
Dissipation Factor 0.00010 - 0.00030
0.00010 - 0.00030
FEP Component