Material Notes:
Papers made from POLYFLON PTFE papers are manufactured from POLYFLON PTFE fibrous powder, and do not contain any other substances. This paper is soft, elastic, and has very low gas permeability. POLYFLON PTFE papers are used as a filter for corrosive liquids, diaphragms for metal plating, and for separation of oil for oil and water mixtures.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Porosity 75 %
75 %
Average, by volume
Thickness 920.0 microns
36.22 mil
Average
Pore Size <= 20.0 microns
<= 0.787 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.50 MPa
218 psi
Average
Elongation at Break 75 %
75 %
Average
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
PTFE Component
Oxygen Index >= 95 %
>= 95 %
PTFE Component
Electrical Properties Metric English Comments
Dielectric Constant 1.9 - 2.1

@Frequency 1000 Hz
1.9 - 2.1

@Frequency 1000 Hz
PTFE Component; ASTM D150
1.9 - 2.1

@Frequency 1e+6 Hz
1.9 - 2.1

@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.00022
0.00010 - 0.00022
PTFE Component