Material Notes:
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is a good bearing material on soft metals & in high speed contact.Chemical: Dynamic & shaft seals; Construction; Bridge bearings; and Slide bearings. Engineering: Anti - friction bearing cages & bearing plates; Bearings, bushes, shaft bearings / seals (in combustion engines); Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology: Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, some fluorine compounds & halogen gases at elevated temperatures.Information provided by Dalau
Physical Properties Metric English Comments
Density 2.10 - 2.18 g/cc
0.0759 - 0.0788 lb/in³
BS2782:Pt6
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 67
65 - 67
ASTM D2240
Tensile Strength 13.5 - 25.0 MPa
1960 - 3630 psi
Moulding Direction; BS2782:Pt3
Elongation at Break 120 - 250 %
120 - 250 %
Moulding Direction; BS2782:Pt3
Thermal Properties Metric English Comments
Thermal Conductivity 0.780 W/m-K
5.41 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Melting Point 327 °C
621 °F
ASTM D3417
Maximum Service Temperature, Air 260 °C
500 °F
300 °C
572 °F
Short Periods
Minimum Service Temperature, Air -200 °C
-328 °F
Flash Point 630 °C
1170 °F
ASTM D1929
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
ASTM D257
Descriptive Properties Value Comments
Color Dark Grey