Denka VINYKON R4105 PVC, R grade for hard extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON R4105 PVC, R grade for hard extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.421 g/cc
0.05134 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.45 MPa
7897 psi
JIS-K-6740
Elongation at Break 167 %
167 %
JIS-K-6740
Flexural Strength 66.0 MPa
9570 psi
JIS-K-6740
Flexural Modulus 2.54 GPa
368 ksi
JIS-K-6740
Izod Impact, Notched 0.47088 J/cm

@Temperature -20.0 °C
0.88215 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
1.295 J/cm

@Temperature 0.000 °C
2.426 ft-lb/in

@Temperature 32.0 °F
JIS-K-6740
2.815 J/cm

@Temperature 23.0 °C
5.275 ft-lb/in

@Temperature 73.4 °F
JIS-K-6740
Penetration 80
80
[°C], penetration temperature; JIS-K-6740
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
JIS-K-6740
Descriptive Properties Value Comments
Thermostability, min, JIS-K-6723 102