Diamond Polymers ASA S-170 Lt Grey 50283UV f1 ASA Weatherable Polymers Injection Molding Grade, High Impact

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA S-170 Lt Grey 50283UV f1 ASA Weatherable Polymers Injection Molding Grade, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.136 GPa
309.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 3.204 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.002 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C

@Load 1.00 kg,
Thickness 3.17 mm
219 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in