Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASA TWP 121

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA TWP 121.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Melt Flow 2.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
chs 2 in/min; ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
Procedure B, Test Method I(chs 0.05 in/min); ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 93.9 °C
201 °F
0.125 inch, 1 Kg; ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
Transmission, Visible 88 %
88 %
Copyright © lookpolymers.com All Rights Reserved