Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASAPC TA-45

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASAPC TA-45.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Melt Flow 12 g/10 min

@Load 10.0 kg,
Temperature 220 °C
12 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.9 MPa
7090 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.549 GPa
369.7 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.01 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C

@Load 1.00 kg,
Thickness 3.17 mm
225 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved