Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY 1001 CF40 40% Carbon Fiber Filled ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 40% Carbon Fiber Filled
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 1001 CF40 40% Carbon Fiber Filled ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.14 %
0.14 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 131 MPa
19000 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 1.0 %
1.0 %
chs 2.0 in/min; ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 19.292 GPa

@Thickness 3.17 mm
2798.1 ksi

@Thickness 0.125 in
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
0.125";; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Users viewing this material also viewed the following: