Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY 173U PC/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 173U PC/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.35 %

@Temperature 23.0 °C
0.35 %

@Temperature 73.4 °F
at equilibrium; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 260 °C
35 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 27 %
27 %
ASTM D638
Flexural Modulus 2.34 GPa
339 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256