Diamond Polymers DIAMALOY 801 Polycarbonate/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 801 Polycarbonate/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 11.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
11.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.2 MPa
8440 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 4.5 %
4.5 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.274 GPa
329.8 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 7.102 J/cm

@Thickness 3.17 mm
13.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 119 °C

@Load 1.00 kg,
Thickness 3.17 mm
246 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1527