Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer

Category Polymer , Thermoplastic , Polystyrene (PS) , Styrene/Methyl Methacrylate Copolymer (SMMA)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 9.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
26.9 g/10 min

@Load 3.80 kg,
Temperature 230 °C
26.9 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength at Break 28.6 MPa
4150 psi
chs 2.0 in/min; ASTM D882
Elongation at Break 54 %
54 %
chs 2.0 in/min; ASTM D882
Flexural Modulus 1.86 GPa
270 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.346 J/cm

@Thickness 3.17 mm
0.648 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 89 %
89 %