Diamond Polymers NPP 60-3302 Clear Polyester Copolymer

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP 60-3302 Clear Polyester Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Viscosity Measurement 0.790
0.790
Intrinsic Viscosity; ASTM D4603
Melt Flow 112 g/10 min

@Load 1.20 kg,
Temperature 300 °C
112 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.2 MPa
8590 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 41 %
41 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 2.577 GPa
373.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Gardner Impact >= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified