Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 6.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.9 MPa
2600 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 6.5 %
6.5 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 0.8475 GPa
122.9 ksi
ASTM D790
Izod Impact, Notched 6.62 J/cm

@Thickness 3.17 mm
12.4 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648