Diamond Polymers NPP25-0802 30G Chemically Couple Glass Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-0802 30G Chemically Couple Glass Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 4.483 GPa
650.2 ksi
ASTM D790
Izod Impact, Notched 0.972 J/cm

@Thickness 3.17 mm
1.82 ft-lb/in

@Thickness 0.125 in
ASTM D256
Descriptive Properties Value Comments
Glass Content (%) 30
ASTM D2584