Diamond Polymers NPP25-1503 GF10 Glass Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 10% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-1503 GF10 Glass Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D792
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 8.7 %
8.7 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 1.685 GPa
244.4 ksi
ASTM D790
Izod Impact, Notched 1.549 J/cm

@Thickness 3.17 mm
2.902 ft-lb/in

@Thickness 0.125 in
ASTM D256
Gardner Impact 1.90 J

@Temperature -20.0 °C
1.40 ft-lb

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
0.125";; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
0.125";; ASTM D648