Diamond Polymers NPP30-0400 MGF30 30% Mineral & Glass Filled Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP30-0400 MGF30 30% Mineral & Glass Filled Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Filler Content 28 - 32 %
28 - 32 %
ASTM D2584
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 5.241 GPa
760.1 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.17 mm
0.806 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
0.125";; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 117 °C
243 °F
0.125";; ASTM D648