Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP50-0355 High Density Polyethylene Blow Molding/Extrusion Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade , High Density Polyethylene (HDPE), Extruded
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP50-0355 High Density Polyethylene Blow Molding/Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR Blow Molding 35 hour
35 hour
Condition B, F50; ASTM D1693
45 hour
45 hour
Condition A, F50; ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
chs 2.0 in/min; ASTM D638
Elongation at Break >= 600 %
>= 600 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 1.378 GPa
199.9 ksi
chs 0.05 in/min; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Users viewing this material also viewed the following: