Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Izod Impact, Notched 6.68 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
ASTM D648