Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
5.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 79.2 MPa
11500 psi
ASTM D638
Flexural Modulus 3.617 GPa
524.6 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.401 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C

@Load 1.00 kg,
Thickness 3.17 mm
225 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified