Material Notes:
Information provided by Domo.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 33 g/10 min
33 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.20 GPa
174 ksi
ISO 527-2
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -30.0 °C
1.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A