Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow 5D98 Polypropylene Homopolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 5D98 Polypropylene Homopolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewConsistent processabilityGood optical propertiesHigh strength propertiesComplies with: U.S. FDA 21 CFR 177.1520 (c)1.1a, Europe EU-Directive 2002/72/ECDOW 5D98 Polypropylene Resin is intended for use in oriented (OPP) film processes.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 3.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790A
Izod Impact, Notched 0.347 J/cm
0.650 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: