Material Notes:
OverviewConsistent processabilityGood color stabilityHigh strength propertiesLow water "carry-over"High speed processingComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW 5E89 Polypropylene Resin is intended for use in stretched tape (raffia) processes, from which the raffia is used to produce woven fabrics for carpet backing, sacking, industrial and geotextile applications.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus, 1% Secant 1380 MPa
200000 psi
ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved