Dow 6D83K Polypropylene Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 6D83K Polypropylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 1.9 g/10 min

@Temperature 230 °C
1.9 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 10 %
10 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 2.94 J/cm
5.50 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648