Dow AFFINITY™ EG 8150 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ EG 8150 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® EG 8150 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It exhibits excellent heat aging and compression set when crosslinked, excellent weatherability. It is also highly effective as an impact modifier in polyolefins, exhibiting superior impact properties in blends with PE and PP.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.868 g/cc
0.0314 lb/in³
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Ratio I10/I2 = 7.7
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Tensile Strength at Break 11.0 MPa
1600 psi
Tensile stress at break.
Elongation at Break 880 %
880 %
100% Modulus 0.00280 GPa
0.406 ksi