Dow AFFINITY™ KC 8852 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ KC 8852 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® KC 8852 polyolefin elastomer is an ethylene-octene copolymer as for one sided stretch cling film in industrial collation packaging. It exhibits excellent inherent cling and optics while offering outstanding toughness.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.875 g/cc
0.0316 lb/in³
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F