Dow AFFINITY™ PF 1140 Polyolefin Plastomer

Category Polymer , Film , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ PF 1140 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fresh produce bags. AFFINITY PF 1140 polymer offers excellent low temperature seal initiation and ultimate hot tack strength in addition to excellent abuse resistance, outstanding optics and high oxygen transmission rates. AFFINITY PF 1140 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. AFFINITY PF 1140 polymer complies with FDA regulation 21 CFR 177.1520c3.1b, which allows for its use in direct food contact applications.Film properties below based on a film thickness of 51 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
Thickness 51.0 microns
2.01 mil
Melt Flow 1.6 g/10 min

@Load 2.16 kg
1.6 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 10.2.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
Film Elongation at Break, TD 710 %
710 %
Elmendorf Tear Strength MD 300 g
300 g
Elmendorf Tear Strength TD 670 g
670 g
Elmendorf Tear Strength, MD 5.90 g/micron
150 g/mil
Elmendorf Tear Strength, TD 13.1 g/micron
333 g/mil
Dart Drop >= 16.3 g/micron
>= 414 g/mil
Film Tensile Strength at Break, MD 49.0 MPa
7110 psi
Film Tensile Strength at Break, TD 43.4 MPa
6290 psi
Optical Properties Metric English Comments
Haze 1.3 %
1.3 %
Processing Properties Metric English Comments
Processing Temperature 81.0 °C
178 °F
Seal initiation temperature
204 °C
399 °F
Film extrusion temperature