Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ultimate seal strength, adhesion to Oriented Polypropylene (OPP) and good taste and odor performance.Information provided by Dow
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Thickness >= 7.62 microns
>= 0.300 mil
Coating Thickness; Extrusion Coating Processability; Dow Method
Melt Index of Compound 7.5 g/10 min
7.5 g/10 min
ASTM D1238
Neck In 13.5 cm
5.31 in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Coating Weight >= 7.20 g/m²
>= 4.50 lb/ream
Extrusion Coating Processability; Dow Method
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.03 MPa
730 psi
to Oriented Polypropylene (OPP) @ 600°F, 1.0 mil coating onto 50 lb Kraft paper; Dow Method
7.17 MPa
1040 psi
to Oriented Polypropylene (OPP) @ 550°F, 1.0 mil coating onto 50 lb Kraft paper; Dow Method
Heat Seal Strength Initiation Temperature 83.0 °C
181 °F
1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method
Thermal Properties Metric English Comments
Melting Point 98.0 °C
208 °F
Dow Method (DSC)
Vicat Softening Point 77.0 °C
171 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 288 - 315 °C
550 - 599 °F
Extrusion Coating Processability