Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Dow Chemical
Trade Name ATTANE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance monolayer blown film or as part of a multilayer film. It has low levels of slip and antiblock additives. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a for food contact.Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.913 g/cc
0.0330 lb/in³
Thickness 38.0 microns
1.50 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.2.
Mechanical Properties Metric English Comments
Coefficient of Friction 0.17
0.17
Elmendorf Tear Strength MD 673 g
673 g
Elmendorf Tear Strength TD 883 g
883 g
Elmendorf Tear Strength, MD 17.7 g/micron
450 g/mil
Elmendorf Tear Strength, TD 23.2 g/micron
589 g/mil
Dart Drop >= 21.8 g/micron
>= 554 g/mil
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
Processing Properties Metric English Comments
Processing Temperature 225 °C
437 °F
Film extrusion temperature