Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow C705-44NA Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C705-44NA Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW C705-44NA Polypropylene Resin is a high melt flow rate impact copolymer that combines superior stiffness and good impact resistance. The product is intended for use in injection molding applications, such as thin wall containers, housewares, and consumer durables.Main CharacteristicsHigh stiffnessNucleated for fast set-upGood impact resistanceContains antistat for mold releaseComplies with U.S. FDA FCN 843Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 44 g/10 min

@Load 2.16 kg,
Temperature 230 °C
44 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.9 MPa
3180 psi
ASTM D638
Flexural Modulus, 1% Secant 1370 MPa
199000 psi
ASTM D790A
Izod Impact, Notched 0.320 J/cm

@Temperature -20.0 °C
0.599 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.374 J/cm

@Temperature 0.000 °C
0.701 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
Unannealed; ASTM D648