Material Notes:
DOW C719-35RNHP is intended for use in injection molding applications requiring a good impact/stiffness balance.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Temperature 230 °C
35 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 5.0 %
5.0 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648