Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning 2-8197 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-8197 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning 2-8197 Emulsion is a non-ionic emulsion of a reactive aminofunctional polydimethylsiloxane suitable to provide a "Fabric Care" benefit for rinse cycle fabric softeners. The use of this product provides water absorbency, ease of wrinkle removal, anti-wrinkle, and ease of ironing when compared to conventional rinse cycle fabric softener compositions.Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 35 %
35 %
Particle Size <= 0.40 µm
<= 0.40 µm
pH 4.5 - 6.5
4.5 - 6.5
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Non-Ionic yes
Water Absorbing yes
Users viewing this material also viewed the following: