Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning 3631 PART A&B KIT

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3631 PART A&B KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, solvent free, heat-cured liquid silicone rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 90000 cP
90000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 19
19
Tensile Strength, Ultimate 5.000 MPa
725.2 psi
Elongation at Break 800 %
800 %
Modulus of Elasticity 0.000280 GPa
0.0406 ksi
at 150% elongation
Tear Strength 16.0 kN/m
91.4 pli
Processing Properties Metric English Comments
Cure Time 0.250 min

@Temperature 130 °C
0.00417 hour

@Temperature 266 °F
0.500 min

@Temperature 110 °C
0.00833 hour

@Temperature 230 °F
2.50 min

@Temperature 80.0 °C
0.0417 hour

@Temperature 176 °F
Pot Life 45 min
45 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance clear
Mix Ratio (X:1) 100
Base to Catalyst ETN
Users viewing this material also viewed the following: