Dow Corning 556 Cosmetic Grade Fluid

Category Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 556 Cosmetic Grade Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A polyphenylmethylsiloxane for use in skincare, suncare, color cosmetic, hair care, and antiperspirant / deodorant applications. INCI Name: Phenyl TrimethiconeInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity Measure 22.5 cSt
22.5 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Closed cup
Optical Properties Metric English Comments
Refractive Index 1.46
1.46