Dow Corning 7355 ADHESIVE

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 7355 ADHESIVE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® 7355 Adhesive is a dispersion of polydimethylsiloxane gum and resin; is blendable with a variety of other dimethyl type silicone PSA's. Provides excellent balance of adhesion and tack, high temperature stability, high adhesion, high performance and negligible silicone volatiles (minimal oven dust).Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 26.0 °C
78.8 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 55-58