Dow Corning 805 RESIN

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 805 RESIN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone binder resin for maintenance paints, colored baking enamels, decorative finishes; primarily with metallic pigments. Used alone or blended with Dow Corning® 806A Resin to promote intermediate hardness.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc

@Temperature 25.0 °C
1.01 g/cc

@Temperature 77.0 °F
Volatile Organic Compounds (VOC) Content 503 g/l
503 g/l
Thermal Properties Metric English Comments
Flash Point 27.0 °C
80.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Resin Content (%) 50