Material Notes:
Silicone binder resin for colored baking enamels for space heaters, stoves, etc. Used alone or blended with Dow Corning® 805 Resin to promote intermediate hardness.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc

@Temperature 25.0 °C
1.02 g/cc

@Temperature 77.0 °F
Volatile Organic Compounds (VOC) Content 515 g/l
515 g/l
Viscosity 150 cP
150 cP
dynamic
Thermal Properties Metric English Comments
Flash Point 7.00 °C
44.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Resin Content (%) 50